(1) Fine grain fracture and low plasticity occur mostly in Q345B square tube after cold working. The reason is that during crystallization annealing or normalizing, the heating temperature is low or the holding time is short, which results in the failure of recrystallization of the broken grains in the process of cold working. The remedial measures are as follows: annealing f crystal, or a complete annealing or normalizing treatment.
(2) For medium carbon steel, excessive hardness is mainly due to excessive heating temperature, too fast cooling, or too low isothermal temperature during annealing; in addition, incorrect normalizing treatment is used; for Q345B square tube, underheating or overheating will cause high hardness after annealing, Dad or due to excessive cooling speed, too low isothermal temperature or insufficient time, etc. Remedial measures: Renormalizing treatment, if the organization is qualified, only high hardness, you can carry out a high temperature tempering treatment.
(3) The occurrence of reticulated structure in eutectoid steels with pre-eutectoid ferrite or eutectoid cementite in hypereutectoid steels shows a reticulated distribution along grain boundaries, which significantly reduces the mechanical properties of Q345B square tube material due to the excessive annealing temperature or slow cooling rate. Remedy: After normalizing the hypereutectoid steel, a high temperature tempering should be carried out again to improve the cutting performance.
(4) The first is that the annealing or normalizing heating temperature is too high and the heating time is too long; or the recrystallization time after 5%? 15% deformation and cold processing is too long, which results in the abnormal grain size and the appearance of coarse grain fracture, which directly reduces the mechanical properties and impact toughness. Remedial measures: normalizing or complete annealing for hypoeutectoid steel; normalizing + spheroidizing annealing or normalizing + tempering for hypereutectoid Q345B square pipe; twice normalizing for Q345B square pipe material with grain size 1?2, the first should be higher than normal temperature 50?150 C, but the heating rate should be faster, the time should be shortened as far as possible, and the second should be normal normalizing temperature. Degree.
Graphite carbon appears in high carbon and steel containing silicon and aluminium. The reason is that the heating temperature is too high and the holding time is too long, which causes the cementite to decompose and precipitate graphite. Seriously, it will reduce the strength of the material and increase its brittleness, which is irreversible.